If the corrosion is not too bad, cut it out and make a fabricated patch to repair the hole as shown here. We used a Craftsman home 110-volt MIG welder to carefully stitch-weld the panel back in place, overlapping the welds to complete the repair. Then the excess weld was ground down to finish the metalwork. View Related Article
|
|